A creep test is done at room temperature on a material on a metal alloy wire comprising of 30% Tin, 25% lead and a solid core copper of 40%. The test measures the increase in strain (Pa) over time (hr) while a constant load is applied to the test specimen wire. Fit the following data using quadratic regression and determine the strain for the duration time t= 5.625 hrs. (note use the rounded off coefficient values in calculating the function). (Answers should be in 3 decimal places) fox) xy x3y 0.452 Blank 1 Blank 2 Blank 3 Blank 4 Blank 5 0.724 Blank 6 Blank 7 Blank 8 Blank 9 Blank 10 3 0.918 Blank 11 Blank 12 Blank 13 Blank 14 Blank 15 0.966 Blank 16 Blank 17 Blank 18 Blank 19 Blank 20 5 0.948 Blank 21 Blank 22 Blank 23 Blank 24 Blank 25 Sum x Sum y Sum x? Sum x3 Sum x Sum xy Sum xy Blank 26 Blank 27 Blank 28 Blank 29 Blank 30 Blank 31 Blank 32 Ao = Blank 33; A, = Blank 34; A2 = Blank 35; f(5.625) = Blank 36 2. 4.
A creep test is done at room temperature on a material on a metal alloy wire comprising of 30% Tin, 25% lead and a solid core copper of 40%. The test measures the increase in strain (Pa) over time (hr) while a constant load is applied to the test specimen wire. Fit the following data using quadratic regression and determine the strain for the duration time t= 5.625 hrs. (note use the rounded off coefficient values in calculating the function). (Answers should be in 3 decimal places) fox) xy x3y 0.452 Blank 1 Blank 2 Blank 3 Blank 4 Blank 5 0.724 Blank 6 Blank 7 Blank 8 Blank 9 Blank 10 3 0.918 Blank 11 Blank 12 Blank 13 Blank 14 Blank 15 0.966 Blank 16 Blank 17 Blank 18 Blank 19 Blank 20 5 0.948 Blank 21 Blank 22 Blank 23 Blank 24 Blank 25 Sum x Sum y Sum x? Sum x3 Sum x Sum xy Sum xy Blank 26 Blank 27 Blank 28 Blank 29 Blank 30 Blank 31 Blank 32 Ao = Blank 33; A, = Blank 34; A2 = Blank 35; f(5.625) = Blank 36 2. 4.
Mathematics For Machine Technology
8th Edition
ISBN:9781337798310
Author:Peterson, John.
Publisher:Peterson, John.
Chapter59: Areas Of Rectangles, Parallelograms, And Trapezoids
Section: Chapter Questions
Problem 79A
Related questions
Question
100%
Expert Solution
This question has been solved!
Explore an expertly crafted, step-by-step solution for a thorough understanding of key concepts.
This is a popular solution!
Trending now
This is a popular solution!
Step by step
Solved in 2 steps
Recommended textbooks for you
Mathematics For Machine Technology
Advanced Math
ISBN:
9781337798310
Author:
Peterson, John.
Publisher:
Cengage Learning,
Functions and Change: A Modeling Approach to Coll…
Algebra
ISBN:
9781337111348
Author:
Bruce Crauder, Benny Evans, Alan Noell
Publisher:
Cengage Learning
Algebra & Trigonometry with Analytic Geometry
Algebra
ISBN:
9781133382119
Author:
Swokowski
Publisher:
Cengage
Mathematics For Machine Technology
Advanced Math
ISBN:
9781337798310
Author:
Peterson, John.
Publisher:
Cengage Learning,
Functions and Change: A Modeling Approach to Coll…
Algebra
ISBN:
9781337111348
Author:
Bruce Crauder, Benny Evans, Alan Noell
Publisher:
Cengage Learning
Algebra & Trigonometry with Analytic Geometry
Algebra
ISBN:
9781133382119
Author:
Swokowski
Publisher:
Cengage