In the Table below Data for Mar M 247-a Nickel base superalloy is shown. (1) Plot the steady state strain rate and time to rupture to predict a relationship between the two variables. Provide an equation for the relationship that you see. (2) Give an explanation as to why the fracture elongation is going up with stress.

Elements Of Electromagnetics
7th Edition
ISBN:9780190698614
Author:Sadiku, Matthew N. O.
Publisher:Sadiku, Matthew N. O.
ChapterMA: Math Assessment
Section: Chapter Questions
Problem 1.1MA
icon
Related questions
icon
Concept explainers
Question

In the Table below Data for Mar M 247-a Nickel base superalloy is shown.
(1) Plot the steady state strain rate and time to rupture to predict a relationship between the two
variables. Provide an equation for the relationship that you see.
(2) Give an explanation as to why the fracture elongation is going up with stress.

 

Temperature (°C) Applied Stress
(MPa)
100
100
150
200
250
300
1000
Minimum creep
rate, sec-1
1.3X10-9
2.8x10-9
3.2x10-8
2.8x10-7
1.6x10-6
7.3x10-6
Time to rupture
(hours)
931.3
969.7
94.3
18.8
4.6
1.33
Fracture
elongation %
1.8
4.7
5.1
8.7
7.3
9.1
Transcribed Image Text:Temperature (°C) Applied Stress (MPa) 100 100 150 200 250 300 1000 Minimum creep rate, sec-1 1.3X10-9 2.8x10-9 3.2x10-8 2.8x10-7 1.6x10-6 7.3x10-6 Time to rupture (hours) 931.3 969.7 94.3 18.8 4.6 1.33 Fracture elongation % 1.8 4.7 5.1 8.7 7.3 9.1
Expert Solution
trending now

Trending now

This is a popular solution!

steps

Step by step

Solved in 3 steps with 2 images

Blurred answer
Knowledge Booster
Design Against Fluctuating Loads
Learn more about
Need a deep-dive on the concept behind this application? Look no further. Learn more about this topic, mechanical-engineering and related others by exploring similar questions and additional content below.
Similar questions
  • SEE MORE QUESTIONS
Recommended textbooks for you
Elements Of Electromagnetics
Elements Of Electromagnetics
Mechanical Engineering
ISBN:
9780190698614
Author:
Sadiku, Matthew N. O.
Publisher:
Oxford University Press
Mechanics of Materials (10th Edition)
Mechanics of Materials (10th Edition)
Mechanical Engineering
ISBN:
9780134319650
Author:
Russell C. Hibbeler
Publisher:
PEARSON
Thermodynamics: An Engineering Approach
Thermodynamics: An Engineering Approach
Mechanical Engineering
ISBN:
9781259822674
Author:
Yunus A. Cengel Dr., Michael A. Boles
Publisher:
McGraw-Hill Education
Control Systems Engineering
Control Systems Engineering
Mechanical Engineering
ISBN:
9781118170519
Author:
Norman S. Nise
Publisher:
WILEY
Mechanics of Materials (MindTap Course List)
Mechanics of Materials (MindTap Course List)
Mechanical Engineering
ISBN:
9781337093347
Author:
Barry J. Goodno, James M. Gere
Publisher:
Cengage Learning
Engineering Mechanics: Statics
Engineering Mechanics: Statics
Mechanical Engineering
ISBN:
9781118807330
Author:
James L. Meriam, L. G. Kraige, J. N. Bolton
Publisher:
WILEY