Superalloys have been made of nickel and aluminum. The alloy owes its strength to the formation of an ordered phase, called the gamma-prime phase, in which At atoms are at the corners of a cubic unit cell and Ni atoms are at the face centers. What is the composition (relative numbers of atoms) for this phase of the nickel- aluminum superalloy?

Interpretation Introduction

Interpretation:

The composition of the Aluminium – Nickel super alloy in its gamma – prime phase has to be determined.

Concept introduction:

Super alloy is also known as High Performance Alloy. Super alloys exhibit excellent properties than normal alloys. They have different and unusual structural features, more perfect than the usual crystalline solids. Due to this, they exhibit excellence in their properties. They have high tensile strength, high resistance to deformation when compared to normal alloys.

Super alloys have various phases in their lattice structure. One of them is known as gamma prime phase (γ') . This phase contains the aggregates that provide stability to the alloy. The metal atoms in the super alloy usually occupy cube faces and cube edges in this (γ') phase. Each atom at the edge is shared by eight unit cells. Each atom at the face of a unit cell is shared by two unit cells.

Explanation

Explanation

A cubic unit cell has 8 corners, 6 faces and 12 edges.   An atom occupying a corner of cubic unit cell is shared by eight unit cells. An atom occupying the face is shared by two unit cells.

It is clearly given that Aluminium occupies corners of the cubic unit cell in its super alloy and Nickel occupied faces of the unit cell. Thus, each Al atom is shared by eight unit cells and each Ni atom is shared by two unit cells

Still sussing out bartleby?

Check out a sample textbook solution.

See a sample solution

The Solution to Your Study Problems

Bartleby provides explanations to thousands of textbook problems written by our experts, many with advanced degrees!

Get Started

Chapter 10 Solutions

Show all chapter solutions add
Ch-10 P-1ALQCh-10 P-2ALQCh-10 P-3ALQCh-10 P-4ALQCh-10 P-5ALQCh-10 P-6ALQCh-10 P-7ALQCh-10 P-8ALQCh-10 P-9ALQCh-10 P-10ALQCh-10 P-11ALQCh-10 P-12ALQCh-10 P-13ALQCh-10 P-15QCh-10 P-16QCh-10 P-17QCh-10 P-18QCh-10 P-19QCh-10 P-20QCh-10 P-21QCh-10 P-22QCh-10 P-23QCh-10 P-24QCh-10 P-25QCh-10 P-26QCh-10 P-27QCh-10 P-29QCh-10 P-30QCh-10 P-31QCh-10 P-32QCh-10 P-34QCh-10 P-35QCh-10 P-36QCh-10 P-37ECh-10 P-38ECh-10 P-39ECh-10 P-40ECh-10 P-41ECh-10 P-42ECh-10 P-43ECh-10 P-44ECh-10 P-45ECh-10 P-46ECh-10 P-47ECh-10 P-48ECh-10 P-49ECh-10 P-50ECh-10 P-51ECh-10 P-52ECh-10 P-53ECh-10 P-54ECh-10 P-55ECh-10 P-56ECh-10 P-57ECh-10 P-58ECh-10 P-59ECh-10 P-60ECh-10 P-61ECh-10 P-62ECh-10 P-63ECh-10 P-64ECh-10 P-65ECh-10 P-66ECh-10 P-67ECh-10 P-68ECh-10 P-69ECh-10 P-70ECh-10 P-71ECh-10 P-72ECh-10 P-73ECh-10 P-74ECh-10 P-75ECh-10 P-76ECh-10 P-77ECh-10 P-78ECh-10 P-79ECh-10 P-80ECh-10 P-81ECh-10 P-82ECh-10 P-83ECh-10 P-84ECh-10 P-85ECh-10 P-86ECh-10 P-87ECh-10 P-88ECh-10 P-89ECh-10 P-90ECh-10 P-91ECh-10 P-92ECh-10 P-93ECh-10 P-94ECh-10 P-95ECh-10 P-96ECh-10 P-97ECh-10 P-98ECh-10 P-99ECh-10 P-100ECh-10 P-101ECh-10 P-103ECh-10 P-104ECh-10 P-105ECh-10 P-106ECh-10 P-107ECh-10 P-108ECh-10 P-109ECh-10 P-110ECh-10 P-111AECh-10 P-112AECh-10 P-113AECh-10 P-114AECh-10 P-115AECh-10 P-116AECh-10 P-117AECh-10 P-118AECh-10 P-119AECh-10 P-120AECh-10 P-121AECh-10 P-122AECh-10 P-123AECh-10 P-124AECh-10 P-125AECh-10 P-126AECh-10 P-127AECh-10 P-128AECh-10 P-129AECh-10 P-131CWPCh-10 P-132CWPCh-10 P-133CWPCh-10 P-134CWPCh-10 P-135CWPCh-10 P-136CWPCh-10 P-137CWPCh-10 P-138CWPCh-10 P-139CWPCh-10 P-140CWPCh-10 P-141CPCh-10 P-142CPCh-10 P-143CPCh-10 P-144CPCh-10 P-145CPCh-10 P-146CPCh-10 P-147CPCh-10 P-148CPCh-10 P-149CPCh-10 P-150CPCh-10 P-151CPCh-10 P-152CPCh-10 P-153CPCh-10 P-154CPCh-10 P-155CPCh-10 P-156CPCh-10 P-157IPCh-10 P-158IPCh-10 P-159IPCh-10 P-160MP

Additional Science Solutions

Find more solutions based on key concepts

Show solutions add

What is meant by the precision of a measurement? How is it indicated?

General Chemistry - Standalone book (MindTap Course List)

When blood glucose concentration rises, the pancreas secretes, and when blood glucose levels fall, the pancreas...

Nutrition: Concepts and Controversies - Standalone book (MindTap Course List)

Describe a polysome in bacterial cells.

Biology (MindTap Course List)

2. In healthy men, the hematocrit is about

Cardiopulmonary Anatomy & Physiology

Spherical waves of wavelength 45.0 cm propagate outward from a point source, (a) Explain how the intensity at a...

Physics for Scientists and Engineers, Technology Update (No access codes included)

A tick is a(n) ______. a. parasitoid b. ectoparasite c. endoparasite

Biology: The Unity and Diversity of Life (MindTap Course List)